牌号 C15
欧标钢号 1.0401
对应标准 EN 10277-2-2008
光亮钢制品.交货技术条件.第2部分:一般工程用钢
Bright steel products - Technical delivery conditions - Part 2: Steels for general engineering purposes
归类 碳钢
C15 化学元素成分含量(%)
成分 C Si Mn P S
最小值 0.12 - 0.3 - -
最大值 0.18 0.4 0.8 0.045 0.045
① Steels with improved machinability as a result of the addition of higher sulphur contents up to around 0,10 % S (including resulphurized steels with controlled inclusion content (e.g. Ca-treatment)) (modern method) or lead may be supplied on request. In the first case the upper limit for the manganese content may be increased by 0,15 %.
②Elements not quoted in this table shall not be added intentionally to the steel without the agreement of the purchaser, other than for the purpose of finishing the heat. All reasonable precautions shall be taken to prevent the addition of such elements from scrap or other material used in the manufacture which affect the hardenability, mechanical properties and applicability.
近似对照表 优质碳素结构钢
中国 德国 法国 欧标
GB DIN EN/DIN NF EN/NF EN 数字牌号
15 C15
Ck15
XC12 C15 1.0401
C15 对应不同标准
1 DIN 17210-1986 渗碳钢.交货技术条件
2 JIS G 7401-2000 冷镦及冷挤压钢
3 ISO 4954-1993 冷镦和冷挤压用钢
4 EN 10277-2-2008 光亮钢制品.交货技术条件.第2部分:一般工程用钢
5 DIN 1652-1963 光亮非合金钢技术供货条件
6 Q/BQB 360-2009 表面硬化钢热连轧钢板及钢带
C15
7 UNI 8550-1984 表面硬化用锻造非合金和合金钢成品—质量、试验要求
8 Q/BQB 130-2003 初轧板坯
C15
注:数据仅供参考!如有疑问,请填写"我要纠错"!
版权说明:
⑴ 本网站的所有内容(包括但不限于文字、图片、音频、视频等)均受到版权保护,版权归本网站所有;
⑵ 未经授权,禁止以任何形式转载、复制、传播或用于其他商业用途;
⑶ 如需使用本网站内容,请提前获得授权。

材料与专利钢号免责声明:
⑴ 本平台所收录的部分材料牌号为企业专利钢号或专有命名牌号,非 GB、ISO、DIN、ASTM、JIS 等通用标准钢号;
⑵ 相关化学成分、力学性能及适用范围以专利文件、权利人公开资料或供方技术文件为准;
⑶ 平台所展示信息仅用于材料检索、工程参考及技术对比,不构成等同、替代或采购依据。
对比 0