牌号 B5
对应标准 BS 3100-1991
一般工程用铸钢件
Specification for Steel castings for general engineering purposes
归类 铸钢
标签 高温用合金钢铸钢
B5 化学元素成分含量(%)
成分 C Si Mn P S Cr Ni Cu Mo
最小值 - - 0.4 - - 4 - - 0.45
最大值 0.2 0.75 0.7 0.04 0.04 6 0.4 0.3 0.65
①碳含量每降低0.01%,最大锰含量则增加0.04%,允许最大锰含量到1.1%
②残余元素。
B5 机械性能
热处理或状态
抗拉强度
σb
Mpa
屈服点
σs
Mpa
断后伸长率或延伸率
δ
%
冲击吸收能量
KV2
J
N+T或OQ+T或WQ+T(T 720°C max) ≥620 ≥420 ≥13 ≥25
A=for anneal by heating to a temperature above the AC3 and cool in the furnace
N=for normalize by heating to a temperature above the AC3 and cool in still air
OQ=for quench into oil from a temperature above the AC3
WQ=for quench into water from a temperature above the AC3
AH=for air harden by heating to a temperature above the AC3 and cool in air at a rate fast enough to produce a hardened microstructure
T=for temper by heating to a temperature below AC1
ST=for solution treat by heating to temperature high enough to dissolve and any intermetallic phases followed by a rapid cool.
如果买方要求对这些等级进行冲击试验,则不进行弯曲试验。
近似对照表 铸钢
日本 美国 德国 英国
JIS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
SCPH32-CF WC9 J21890 GS-12CrMo 9 10 1.7380 625
B5
B5 对应不同标准
1 ASTM A193/A193M-2001 高温设备用合金钢和不锈钢螺栓材料的标准规范
2 GB /T 5231-2012 加工铜及铜合金牌号和化学成分
3 ASTM A485-2014 高淬透性耐磨轴承钢的技术规范
4 ASTM A485-2017 高淬透性耐磨轴承钢的技术规范
5 GB /T 2040-2017 铜及铜合金板材
6 GB /T 5231-2022 加工铜及铜合金牌号和化学成分
7 BS 3100-1991 一般工程用铸钢件