牌号 14MoV6-3
欧标钢号 1.7715
对应标准 EN 10222-2-2017
压力用途用钢制锻件 第2部分 具有高温特性的铁素体和马氏体钢
Steel Forgings for Pressure Purposes. Part 2:Ferritic and Martensitic Steels with Specified Elevated Temperature Properties
归类 合金钢
14MoV6-3 化学元素成分含量(%)
成分 C Si Mn P S Cr Mo V Al Sn
最小值 0.1 - 0.4 - - 0.3 0.5 0.22 - -
最大值 0.18 0.4 0.7 0.025 0.01 0.6 0.7 0.28 0.02 0.025
14MoV6-3 机械性能
厚度
t
mm
抗拉强度
σb
Mpa
屈服点
σs
Mpa
断后伸长率或延伸率
δ
%
冲击吸收能量
KV2
J
t≤500 460~610 ≥300 I:≥20,tr/t:≥18 ≥27
① I = longitudinal to main forging directions;tr = transverse to main forging directions;t = tangential.
② Maximum room temperature for the impact test is 20 °C. By option, impact testing may be carried out at 0°C, with the condition to fulfil the impact values as stated in this table.
③ Until the yield point criteria are harmonized in the various national codes, determination of ReH may be replaced by determination of Rp0.2. In this case Rp0.2 values are 10 MPa lower for ReH values up to 355 MPa and 15 MPa lower for ReH values greater than 355 MPa.

  • 热处理制度(仅供参考)

    QT= quenched and tempered; NT= normalized and tempered. a = air; f = furnaced; o = oil; w = water or water based medium.

14MoV6-3 对应不同标准
1 EN 10222-2-2000 压力用途用钢制锻件 第2部分 具有高温特性的铁素体和马氏体钢
2 EN 10222-2-2017 压力用途用钢制锻件 第2部分 具有高温特性的铁素体和马氏体钢
注:数据仅供参考!如有疑问,请填写"我要纠错"!